Isothermal differential scanning calorimetry (DSC) tests were
performed
on three unsaturated polyester (UPE) samples at three different
temperatures
(100C, 110C, and 120C). The output for the three DSC
tests is presented in the Fig. 4.30. On the graph, label which
curve is
associated with which test temperature. From the curves in Fig.
4.30 estimate
the total heat of reaction, QT.