The Fe-3.5% Si alloy was experienced 60% cold work and then
annealed at different temperatures. The recrystallization data are
reported in Figure 9.32 
a. The activation energy of the recrystallization of Fe-3.5% Si alloy experienced 60% cold work
b. The time required for 50% recrystallization at 350C